Natural charcoal produced traditionally in a clay oven
Made of hardwood, not sparking, and with high calorific value.
- Calorific value: Not less than 6 000 Kcal/Kg
- Maximum humidity allowed: 6%
- Solid carbon: 80-90% • Abrasive: 68%.
- Ash: 2%
- Volatile: 5-10%.
- Incandescence time: 4-5 hours.
- Uniform color.
- Sound: Metallic, does not spark or explode, burns with a smokeless flame. Approximate dimensions